Textile Engineering > GATE 2025 > Yarn Testing
The parameter(s) required to convert load-elongation curve to stress-strain curve of a yarn is/are
A
initial linear density of yarn
B
linear density of yarn at break
C
gauge length of yarn
D
length of yarn at break

Correct : a