Textile Engineering > GATE 2024 > Degree of Crystallinity
Three melt-spun fibre samples A, B and C produced from same polymer under different conditions are found to have densities 1.10 g/cm³, 1.15 g/cm³ and 1.20 g/cm³ respectively. If the mass fraction based degree of crystallinity (xc) of A and C is 0.45 and 0.75, respectively, then xc for B (rounded off to 2 decimal places) is _______.

Correct : 0.60

Similar Questions

Inhaling the smoke from a burning _________ could _________ you quickly.
#2 MCQ
A sphere of radius 𝑟 cm is packed in a box of cubical shape. What should be the minimum volume (in cm3) of the box that can enclose the sphere?
#3 MCQ
Pipes P and Q can fill a storage tank in full with water in 10 and 6 minutes, respectively. Pipe R draws the water out from the storage tank at a rate of 34 l...
#4 MCQ

Related Topics

melt spun fibre density melt spun degree of crystallinity textile engineering gate crystallinity melt spun polymer crystallinity melt spun fibre crystallinity GATE textile engineering 2024 melt spun density crystallinity melt spun engineering

Unique Visitor Count

Total Unique Visitors

Loading......