Textile Engineering > GATE 2021 > Synthetic Fibres
In melt spinning, the mass throughput rate of polymer is 210 g/min, the winding speed is 3000 m/min, and the linear density of the yarn produced is 200 denier. The effective draw ratio, (rounded off to two decimal places), is

Correct : 3.00 to 3.30