Textile Engineering > GATE 2020 > Wet Spinning
In wet spinning of acrylic filament yarn, the volumetric flow rate of the spinning dope per spinneret hole is 0.1 cm³/min. If the surface speed at the first take up roller is 1.5 m/min and the diameter of spinneret hole is 0.02 cm, then the jet stretch (rounded off to 2 decimal places) is

Correct : 0.46 to 0.48