Textile Engineering > GATE 2016 > Fabric Testing
A fabric specimen of original length 75 mm is stretched to a length of 120 mm and after removal of the load the length reduces to 95 mm. The elastic recovery (%) of the fabric specimen is
Correct : 55:56
Similar Questions
A high value of drape coefficient indicates
A woven fabric with areal density of $300g/m2 is tested by strip tensile test method, keeping the specimen width as 5 cm and gauge length as 25 cm. If the break...
A fabric with a mass per unit area of 250 g/m² has a flexural rigidity of 275 μN⋅m. What is the bending length (in mm) of the fabric, rounded off to two decimal...