Textile Engineering > GATE 2014 > Melt Spinning
A polypropylene yarn, melt spun at a throughput rate of W (g/s) and winding speed of S (m/min), was drawn to a draw ratio of D. The denier of this yarn is a function of W, S, D and a constant K. The value of K, accurate to the nearest integer, is

Correct : 540000 to 540000

Similar Questions

Determine the correctness or otherwise of the following Assertion [a] and Reason [r]: [a]: Nylon 6 should be thoroughly dried before melt spinning [r]: The gl...
#47 MCQ
In melt spinning of a monofilament, a polymer is being extruded at a volumetric flow rate of 5 × 10⁻⁵ m³/s through a spinneret of circular cross-section. If the...
#131 Fill in the Blanks
In melt spinning of poly(ethylene terephthalate), pre-drying of polymer chips is essential to avoid
#289 MCQ

Related Topics

polypropylene yarn draw spinning GATE Textile Engineering 2014 yarn denier calculation melt spun yarn draw ratio yarn textile engineering gate spinning yarn denier yarn spinning engineering GATE 2014 Textile Engineering

Unique Visitor Count

Total Unique Visitors

Loading......