Textile Engineering > GATE 2013 > Textile Finishing
Consider the following assertion [a] and reason [r] and choose the most appropriate answer.
[a] Controlled reduction treatments are commercially used for shrink resist finishing of wool
[r] Reduction disrupts the disulphide bonds, which are responsible for wool shrinkage
A
[a] is right [r] is wrong
B
[a] is right [r] is right
C
[a] is wrong [r] is wrong
D
[a] is wrong [r] is right

Correct : b

Similar Questions

Dimethylol dihydroxy ethylene urea (DMDHEU) is a
#209 MCQ
The wet expression for a padding mangle is set at 80%. If the add-on of a flame retardant chemical required on the fabric is 2% then the concentration (g/L) of...
#220 NAT
Determine the correctness or otherwise of the following Assertion [a] and Reason [r] Assertion: Application of an optical brightening agent makes the white fab...
#235 MCQ

Related Topics

controlled reduction treatments shrink resistant wool disulphide bonds GATE textile engineering 2013 reduction disrupts bonds wool shrinkage textile engineering gate disulphide bonds wool