A cylindrical Al alloy billet of 300 mm diameter is hot extruded to produce a cylindrical rod of 75 mm diameter at a constant true strain rate ( ) of 10s-1. The flow stress (σ) of the alloy at the extrusion temperature is given by σ=10(ε̇)0.3 MPa.
Assume the alloy is perfectly plastic and there is no temperature rise during the extrusion process.
The ideal plastic work of deformation per unit volume is ______ ×106 J m-3 (rounded off to one decimal place).
Assume the alloy is perfectly plastic and there is no temperature rise during the extrusion process.
The ideal plastic work of deformation per unit volume is ______ ×106 J m-3 (rounded off to one decimal place).
Correct : 0.3
Similar Questions
Match the defects in Column I with corresponding metal forming techniques in Column II.
In rolling, the point on the surface of contact between roll and sheet where surface velocity of the roll is equal to velocity of the sheet is referred as _____...
Mr. X speaks _________ Japanese _________ Chinese.
Total Unique Visitors
Loading......