Metallurgical Engineering > GATE 2025 > Steelmaking
Molten steel at 1900 K having dissolved hydrogen needs to be vacuum degassed.
The equilibrium partial pressure of hydrogen to be maintained to achieve 1 ppm (mass basis) of dissolved hydrogen is ______ Torr (rounded off to two decimal places).
Given: For the hydrogen dissolution reaction in molten steel (1/2 H2(g)=[H]), the equilibrium constant (expressed in terms of ppm of dissolved H) is: log10Keq = -1900/T+2.4
1 atm = 760 Torr

Correct : 0.05

Similar Questions

For supersonic O2 jet in basic oxygen furnace steelmaking, choose the correct combination from the following:
#111 MCQ
Which one of the following elements has the slowest removal rate from hot metal in basic oxygen furnace (BOF) steelmaking?
#152 MCQ
The correct sequence of steelmaking operations is _______ [BOF: Basic Oxygen Furnace; LF: Ladle Furnace; VD: Vacuum Degassing; CC: Continuous Casting].