Metallurgical Engineering > GATE 2025 > Casting Defects
Match the casting defects in Column I with the characteristic features in Column II.
Column IColumn II
P. Misrun1. Penetration of liquid metal behind surface layer of sand moulds
Q. Expansion scab2. Metal solidifies prematurely in the mould and some sections of the casting are not filled
R. Pin holes3. Cracking because of restraint to contraction in certain areas of the casting during solidification and cooling to room temperature
S. Hot tearing4. Evolution of gases during solidification resulting in porosity
A
P-2,Q-4,R-3,S-1
B
P-1,Q-3,R-2,S-4
C
P-1,Q-2,S-3,R-4
D
P-2,Q-1,R-4,S-3

Correct : d

Similar Questions

Mr. X speaks _________ Japanese _________ Chinese.
#2 MCQ
A sum of money is to be distributed among P, Q, R, and S in the proportion 5 : 2 : 4 : 3, respectively. If R gets ₹ 1000 more than S, what is the share of Q (...
#3 MCQ
A trapezium has vertices marked as P, Q, R and S (in that order anticlockwise). The side PQ is parallel to side SR. Further, it is given that, PQ = 11 cm, QR...
#4 MCQ

Related Topics

No tags found

Unique Visitor Count

Total Unique Visitors

Loading......