Metallurgical Engineering > GATE 2021 > Kinetics
Nickel undergoes isothermal oxidation at 800 K for a duration of 400 s resulting in a weight gain of 2 mg cm2. The weight gain (mg cm2) after a duration of 1600 s is: _______ (round off to nearest integer). Assume: Weight gain is proportional to square root of time.

Correct : 4

Similar Questions

Which one of the following schematics represents the variation of the rate of nucleation of solid from a pure liquid metal as a function of undercooling (&Delta...
#30 MCQ
For a solid embryo in contact with a perfectly flat mould wall as shown in the schematic, the wetting angle θ is _______ degrees. (Round off to one de...
#41 Fill in the Blanks
A non-porous spherical Fe2O3 particle of initial radius of 5 × 10-2 m is topo-chemically reduced by H2 where the reactant-product interface is sharp and s...
#66 Fill in the Blanks

Related Topics

isothermal oxidation nickel Metallurgical Engineering GATE 2021 weight gain proportional to square root of time oxidation nickel GATE metallurgical engineering time weight gain relationship nickel oxidation GATE 2021 metallurgy oxidation kinetics nickel