Metallurgical Engineering > GATE 2021 > Blast Furnace
A blast furnace uses hematite ore with 80% Fe2O3 and 20% gangue materials. It uses 600 kg coke per ton of hot metal. The coke contains 85% C and 15% ash. The composition of hot metal is 95.5% Fe and 4.5% C. The weight of iron ore used and slag produced per ton of hot metal respectively, are:
Given: Atomic weight: O = 16, C = 12, N = 14, Fe = 56
All the compositions are in wt.%.
1 ton = 1000 kg
Assume that the gangue materials of the ore and ash content of coke form slag while Fe2O3 in the ore is consumed in making hot metal.
A
1705 kg, 431 kg
B
2131 kg, 546 kg
C
1705 kg, 331 kg
D
1500 kg, 431 kg

Correct : a

Similar Questions

Which one of the following modern practices is used for retarding the solution loss reaction in blast furnace ironmaking?
#158 MCQ
A blast furnace charged with hematite containing 90 wt.% Fe₂O₃ produces liquid iron with 3.6 wt.% carbon. Coke containing 90 wt.% carbon is charged at a rate of...
#384 Fill in the Blanks
Which of the following conditions is/are favorable for producing low-silicon hot metal in blast furnace ironmaking?
#426 MCQ

Related Topics

metallurgical engineering gate 2021 blast furnace operation hematite ore coke usage hot metal production slag formation iron ore consumption metallurgy problems iron and steel production metallurgical engineering calculations ore composition analysis coke composition iron ore percentage slag production metallurgy exam questions

Unique Visitor Count

Total Unique Visitors

Loading......