Metallurgical Engineering > GATE 2020 > Fracture Mechanics
A component subjected to tensile stress in a mechanical device is monitored periodically for cracks by NDT. The NDT technique can only detect cracks (both surface and internal) which are larger than 1 mm. Keeping a 10% margin of safety, the maximum allowed tensile stress on the component will be _______ MPa (round off to the nearest integer). Given, fracture toughness KIC = 30 MPa m1/2 and assume crack geometry factor of unity.

Correct : 490

Similar Questions

For a component fabricated from an alloy A with plane strain fracture toughness, KIC=50 MPa m1/2, fracture was observed to take place at a crack length of 0.4 m...
#457 NAT
For a component fabricated from an alloy A with plane strain fracture toughness, KIC=50 MPa m1/2, fracture was observed to take place at a crack length of 0.4 m...
#457 NAT
For a component fabricated from an alloy A with plane strain fracture toughness, KIC=50 MPa m1/2, fracture was observed to take place at a crack length of 0.4 m...
#457 NAT

Related Topics

No tags found

Unique Visitor Count

Total Unique Visitors

Loading......