Metallurgical Engineering > GATE 2019 > Blast Furnace
A blast furnace charged with hematite containing 90 wt.% Fe₂O₃ produces liquid iron with 3.6 wt.% carbon. Coke containing 90 wt.% carbon is charged at a rate of 500 kg per Metric ton of liquid iron produced. The blast furnace top gas contains (by volume), 22% CO, 18% CO₂, and balance nitrogen. The volume of the blast furnace top gas [in m³ (NTP), rounded off to the nearest integer] is _______.
Given: Assume ideal gas behavior, and molar volume of the gas at NTP is 22.4 liter.

Correct : 1930

Similar Questions

Which one of the following modern practices is used for retarding the solution loss reaction in blast furnace ironmaking?
#158 MCQ
A blast furnace uses hematite ore with 80% Fe2O3 and 20% gangue materials. It uses 600 kg coke per ton of hot metal. The coke contains 85% C and 15% ash. The co...
#245 MCQ
Which of the following conditions is/are favorable for producing low-silicon hot metal in blast furnace ironmaking?
#426 MCQ

Related Topics

blast furnace design hematite to iron conversion coke carbon content GATE Metallurgical Engineering 2019 blast furnace top gas ideal gas behavior molar volume gas blast furnace gas volume metallurgical engineering gate

Unique Visitor Count

Total Unique Visitors

Loading......