Metallurgical Engineering > GATE 2019 > Fracture Strength
The length of internal cracks in two samples of the same glass is measured to be c₁ = 0.5 mm and c₂ = 2 mm. The ratio (σ₁ / σ₂) of the fracture strength of the two samples is _______.
A
0.5
B
1.0
C
2.0
D
4.0

Correct : c