Mechanical Engineering > GATE 2025 > Fatigue Design
The endurance limit of a specific grade of steel is same as its yield strength. The ultimate strength of this grade of steel is twice of its yield strength. A component made of this steel is loaded in tension and unloaded periodically. It is required that the component does NOT fail for at least 106 loading cycles, as per the Soderberg law. Considering a factor of safety of 2, the maximum applied tensile principal stress is
Correct : b
Similar Questions
A bar is subjected to fluctuating tensile load from 20 kN to 100 kN. The material has yield strength of 240 MPa and endurance limit in reversed bending is 160 M...
A bar is subjected to fluctuating tensile load from 20 kN to 100 kN. The material has yield strength of 240 MPa and endurance limit in reversed bending is 160 M...
A machine element has an ultimate strength (σu) of 600 N/mm2, and endurance limit (σen) of 250 N/mm2. The fatigue curve for the element on a log-log plot is sho...