Two mild steel plates of similar thickness, in butt-joint configuration, are welded by gas tungsten arc welding process using the following welding parameters:
The filler wire feed rate is selected such that the final weld bead is composed of 60% volume of filler and 40% volume of plate material. The heat required to melt the mild steel material is 10 J/mm³. The heat transfer factor is 0.7 and melting factor is 0.6. The feed rate of the filler wire is __________ mm/s (round off to one decimal place).

Correct : 3.5

Similar Questions

The most suitable electrode material used for joining low alloy steels using Gas Metal Arc Welding (GMAW) process is
#189 MCQ
In an arc welding process, the voltage and current are 30 V and 200 A, respectively. The cross-sectional area of the joint is 20 m m 2 and the welding speed is...
#206 Fill in the Blanks
In an direct current arc welding process, the power source has an open circuit voltage of 100 V and short circuit current of 1000 A. Assume a linear relations...
#372 Fill in the Blanks

Related Topics

butt joint welding GATE Mechanical Engineering 2022 gas tungsten arc welding mild steel butt joint weld bead composition heat transfer factor mechanical engineering welding parameters selection GATE set 1 question 57 filler wire feed rate calculation mechanical engineering gate welding process parameters

Unique Visitor Count

Total Unique Visitors

Loading......