Mechanical Engineering > GATE 2014 SET-3 > Manufacturing Technology
The hot tearing in a metal casting is due to
A
high fluidity
B
high melt temperature
C
wide range of solidification temperature
D
low coefficient of thermal expansion

Correct : c

Similar Questions

The process utilizing mainly thermal energy for removing material is
#522 MCQ
A straight turning operation is carried out using a single point cutting tool on an AISI 1020 steel rod. The feed is 0.2 mm/rev and the depth of cut is 0.5 mm....
#524 Fill in the Blanks
Match the casting defects (Group A) with the probable causes (Group B):Group AP: Hot tearsQ: ShrinkageR: Blow holesS: Cold ShutGroup B1: Improper fusion of two...