Mechanical Engineering > GATE 2014 SET-2 > Metal Forming
A mild steel plate has to be rolled in one pass such that the final plate thickness is 2/3rd of the initial thickness, with the entrance speed of 10 m/min and roll diameter of 500 mm. If the plate widens by 2% during rolling, the exit velocity (in m/min) is _______

Correct : 14.7

Similar Questions

The size distribution of the powder particles used in Powder Metallurgy process can be determined by
#46 MCQ
The "Earing" phenomenon in metal forming is associated with
#186 MCQ
A 4 mm thick aluminum sheet of width w = 100 mm is rolled in a two-roll mill of roll diameter 200 mm each. The workpiece is lubricated with a mineral oil, wh...
#316 Fill in the Blanks

Related Topics

No tags found

Unique Visitor Count

Total Unique Visitors

Loading......