Civil Engineering > GATE 2022 SET-2 > Prestressed Concrete
A post-tensioned concrete member of span 15 m and cross-section of 450 mm ร— 450 mm is prestressed with three steel tendons, each of cross-sectional area 200 mm2. The tendons are tensioned one after another to a stress of 1500 MPa. All the tendons are straight and located at 125 mm from the bottom of the member. Assume the prestress to be the same in all tendons and the modular ratio to be 6. The average loss of prestress, due to elastic deformation of concrete, considering all three tendons is ________ MPa.
A
14.16
B
7.08
C
28.32
D
42.48

Correct : a

Similar Questions

In a pre-stressed concrete beam section shown in the figure, the net loss is 10% and the final pre-stressing force applied at X is 750 kN. The initial fiber str...
#1401 MCQ
In a pre-stressed concrete beam section shown in the figure, the net loss is 10% and the final pre-stressing force applied at X is 750 kN. The initial fiber str...
#1401 MCQ
In a pre-stressed concrete beam section shown in the figure, the net loss is 10% and the final pre-stressing force applied at X is 750 kN. The initial fiber str...
#1401 MCQ

Related Topics

No tags found

Unique Visitor Count

Total Unique Visitors

Loading......